    7075-T6 has a much higher tensile strength and is harder than 6061-T6.
    7075-T6 aluminum has a higher tensile strength and is harder than 660 bronze bearing

    7075-T6 principal alloying ingredients are Zinc and copper, which make it one of the highest-strength aluminum alloys that are available.
    In fact, its typical strength in the T6 temper is higher than most mild steels.

    7075-T6 Aluminum
    Physical and Mechanical Properties   Ultimate Tensile Strength, psi   83,000
    Yield Strength, psi   73,000
    Brinell Hardness   150
    Rockwell Hardness   B87

    6061-T6 Aluminum
    Physical and Mechanical Properties   Ultimate Tensile Strength, psi   45,000
    Yield Strength, psi   40,000
    Brinell Hardness   95
    Rockwell Hardness   B60

    Bronze Bearing


    Bearing Bronze (C932), a/k/a SAE 660
    Minimum Properties   Ultimate Tensile Strength, psi   35,000
    Yield Strength, psi   20,000
    Brinell Hardness   65



    Aluminum Bronze, C954
    Minimum Properties    Ultimate Tensile Strength, psi    85,000
    Yield Strength, psi    32,000
    Elongation in 2"    12%
    Brinell Hardness    170

    On voit que l'aluminium bronze C954 est bien placé ,ce qui me conforte dans mon choix.

    We see that bronze aluminum C954 is well placed, which confirms my choice.

    Vemos que el bronce-aluminio C954 está bien posicionado, lo cual me reafirma en mi elección.

    « Article publié depuis OverBlog »
    Partager via Gmail Delicious Technorati Yahoo! Google Bookmarks Blogmarks

  • Commentaires

    Aucun commentaire pour le moment

    Suivre le flux RSS des commentaires


    Ajouter un commentaire

    Nom / Pseudo :

    E-mail (facultatif) :

    Site Web (facultatif) :

    Commentaire :